| 弹性漆对消光粉的要求 |
| 添加时间:2019/9/28 15:19:16 浏览次数: |
| 弹性漆对消光粉的要求有: Elastic paints require matting powder as follows: (1)消光性,要求在添加量6~7%时候消到10度以下 (1) Extinction, which should be reduced to less than 10 degrees when the dosage is 6-7%. (2)手感,对手感要求较高 (2) Hand feeling, higher requirement for hand feeling (3)防沉性:由于对透明度要求较高,一般不加防沉剂 (3) Anti-sedimentation: Because of the high requirement for transparency, no anti-sedimentation agent is usually added. (4)透明度,在添加量6~7%不会发白,手掐不会留下白色的痕迹 (4) Transparency, 6-7% of the added amount will not whiten, hand pinch will not leave white marks. |
| 上一页 什么是消光效果? |
| 下一页 消光粉光泽和光泽的测定 |